What causes the matt surface of PVC plastic pipes

2019-11-01 1406

When the surface of PVC plastic pipe is Matt, the reasons are as follows:

The first reason may be that the die temperature is too low, which can be treated by increasing the die temperature and adding ACR dosage to improve the shearing;

The second reason may be that the shear rate is too high and the melt breaks. We can solve this problem by properly increasing the feed temperature, increasing the amount of ACR or decreasing the traction speed;

The third reason may be that the die temperature is too high or the internal surface finish is poor. We can solve this problem by reducing the die temperature and its roughness;

PVC工程塑料

The fourth reason may be that the plasticizing of plastic additives is poor. We can solve this problem by improving the temperature and adding processing additives;

The fifth reason may be that the content of external lubricant is too low. We can properly add external lubricant. Of course, this is to ensure that the material is plasticized;

Sixth, perhaps because the particle size of CaCO3 is too large or the particle size distribution is too wide, now we can replace the applicable calcium carbonate to deal with this problem.